    Behavioral modeling of clock feed-through and channel charge injection non-ideal effects in SIMULINK for switched-capacitor integrator

    , Article Simulation Modelling Practice and Theory ; Volume 18, Issue 5 , May , 2010 , Pages 483-499 ; 1569190X (ISSN) Torkzadeh, P ; Atarodi, M ; Sharif University of Technology
    2010
    Abstract
    Sigma-Delta modulator ADCs used in signal processing applications usually, are implemented by switched-capacitor (SC) circuits and CMOS transmission gates due to its simplicity for implementation. Channel charge injection (CCI) and clock feed-through (CFT) are two major non-ideal effects existing in TG switches and SC integrators reducing modulator total SNR, its linearity and its total gain. This paper presents a precise model for SC integrator including CCI and CFT non-ideal effects in MATLAB SIMULINK environment which allows designers to perform time-domain behavioral simulations of switched-capacitor (SC) Sigma-Delta modulators. Evaluation and validation of extracted models were... 

    Investigating the different conditions on solution processed MoOx thin film in long lifetime fluorescent polymer light emitting diodes

    , Article Materials Chemistry and Physics ; Volume 204 , 2018 , Pages 262-268 ; 02540584 (ISSN) Alehdaghi, H ; Marandi, M ; Irajizad, A ; Taghavinia, N ; Jang, J ; Zare, H ; Sharif University of Technology
    Elsevier Ltd  2018
    Abstract
    Transition metal oxides are being more frequently used as hole injection layer (HIL) in organic light emitting diodes (OLEDs), in place of polymer HILs such as PEDOT:PSS. The very thin films of the metal oxide HILs are usually deposited using vapor deposition, in order to create uniform films. Here, we report OLEDs fabricated using solution processed MoOx films as the HIL and super yellow as the emissive layer. The performance of the devices is comparable to PEDOT:PSS based devices, while the stability tests show the lifetime of MoOx-based devices is 4 × 106 h, about 40 times longer than PEDOT:PSS devices, at typical working condition. X-ray photoelectron spectroscopy (XPS) indicates both...