Comparison of different strategies for the assembly of gold colloids onto Fe3O4@SiO2 nanocomposite particles
, Article Physica E: Low-Dimensional Systems and Nanostructures ; Volume 49 , 2013 , Pages 30-38 ; 13869477 (ISSN) ; Yaghmaei, S ; Roostaazad, R ; Arpanaei, A ; Sharif University of Technology
2013
Abstract
Three strategies were employed for the assembly of gold nanoparticles on silica-coated magnetite particles (SCMPs). In strategy I, citrate-coated gold nanoparticles were attached on the surface of amine-SCMPs. In strategy II, amine-SCMPs were coated with carboxylated gold nanoparticles via amide bond formation. In strategy III, the thiol-SCMPs surface was coated with gold nanoparticles. Among the above examined strategies, coating amine-SCMPs with gold nanoparticles via strategy I resulted in a better coverage and stronger intensity of absorption bands. Furthermore, results obtained through strategy I showed that decreasing the pH of the solution from 7 to 3 leads to a further red-shift of...
Characterization and calcination behavior of a low-grade manganese ore
, Article Materials Today Communications ; Volume 25 , 2020 ; Becker, H ; Eftekhari, H ; Yoozbashizadeh, H ; Safarian, J ; Sharif University of Technology
Elsevier Ltd
2020
Abstract
Characterization and calcination behavior of a low-grade manganese ore, as a part of Mn ferroalloys production, was studied by XRF, ex-situ XRD, in-situ XRD, and SEM-EDS techniques. Calcination experiments were carried out at and up to 900 °C (1173 K) in air and argon atmospheres. The samples were in particles and powder forms. The results indicated that both quartz and calcite phases in the ore exhibit a bimodal spatial distribution; as relatively large regions and finely distributed in the Mn- and Fe-containing phases. By Rietveld analysis of the in-situ XRD data, the reactions occurring upon heating during the calcination process were deduced. Thermal decomposition and reactive diffusion...