Loading...
Search for: mass-loss
0.004 seconds

    Thermal degradation behavior and kinetic analysis of ultra high molecular weight polyethylene based multi-walled carbon nanotube nanocomposites prepared via in-situ polymerization

    , Article Journal of Macromolecular Science, Part A: Pure and Applied Chemistry ; Volume 49, Issue 9 , 2012 , Pages 749-757 ; 10601325 (ISSN) Shariati, J ; Saadatabadi, A. R ; Khorasheh, F ; Sharif University of Technology
    T&F  2012
    Abstract
    Thermal degradation behavior of multi-wall carbon nanotubes (MWCNTs)/ultra high molecular weight polyethylene (UHMWPE) nanocomposites, with different nanotubes contents (0.5, 1.5 and 3.5 wt%) prepared via in-situ polymerization technique have been investigated using thermal gravimetric analysis (TGA). TGA spectra revealed that these nanocomposites had enhanced thermal stability and no significant mass loss (<0.4 wt%) occurred up to 350°C. Thermal degradation of these UHMWPE/MWCNT nanocomposites was investigated in terms of parameters such as the onset temperature of degradation (T 10), the decomposition temperature at 50% wt loss (T 50), the degradation temperature of maximum rate of the... 

    Comparative study on the effect of fiber type and content on the fire resistance of alkali-activated slag composites

    , Article Construction and Building Materials ; Volume 288 , 2021 ; 09500618 (ISSN) Shoaei, P ; Ghassemi, P ; Ameri, F ; Musaeei, H. R ; Chee Ban, C ; Ozbakkaloglu, T ; Sharif University of Technology
    Elsevier Ltd  2021
    Abstract
    Alkali-activated slag (AAS) binder has been recognized as a suitable material for construction applications owing to its low carbon footprint and good mechanical and durability performance. As a promising alternative to the conventional Portland cement binder, it is important to maximize the performance of AAS composites under normal and harsh environmental conditions such as exposure to fire. The use of fibers in a brittle matrix is a well-known approach to enhance the mechanical strength and cracking behavior under thermal loading. In this study, polypropylene fiber (PPF), glass fiber (GF), and basalt fiber (BF) are used at volume fractions of 0.5%, 1%, and 1.5% in AAS mortar mixes. First,...