Densification and microstructural evolution during co-sintering of Ni-base superalloy powders
, Article Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science ; Volume 37, Issue 8 , 2006 , Pages 2549-2557 ; 10735623 (ISSN) ; Sharif University of Technology
2006
Abstract
This work presents the effect of co-sintering on the densification and microstructural evolution in the two-layer stepwise graded composite of INCONEL 718 and INCONEL 625 superalloys. A pressureless co-sintering method in conjunction with a powder layering technique was used. The sintering was carried out in solid state and liquid phase in temperature ranging from 1260 °C through 1300 °C for 60 minutes in a low pressure of an argon atmosphere. Nonisothermal sintering behavior was also examined by dilatometric analysis. Similarly, the sintering response of the individual layers was characterized. The results reveal an enhanced densification rate during co-sintering of the composite layers....