    Crystallization of hydroxyapatite during hydrothermal treatment on amorphous calcium phosphate layer coated by PEO technique

    , Article Ceramics International ; Volume 39, Issue 2 , 2013 , Pages 1793-1798 ; 02728842 (ISSN) Faghihi Sani, M. A ; Arbabi, A ; Mehdinezhad Roshan, A ; Sharif University of Technology
    2013
    Abstract
    Surface modification of titanium implants is recently considered by several researchers. In this study, PEO was performed over commercially Ti-6Al-4V alloy pellets in an aqueous electrolyte containing calcium acetate (C.A.) and calcium glycerphosphate (Ca-GP) with a Ca/P molar ratio of 6.8, and applying current density of 0.212 A/cm2, frequency of 100 Hz and duty ratio of 60% for 4 min. In the next step, hydrothermal treatments were carried out for various durations and at different temperatures inside an autoclave chamber containing a NaOH solution with pH of 11.5. XRD and SEM results confirmed formation of needle-shaped HAp after all hydrothermal conditions. Maximum intensity of HAp peaks... 

    Investigating the effect of rolling strain on fracture behavior of roll bonded Al6061 laminates under quasi-static and dynamic loading

    , Article Materials Science and Engineering A ; Volume 558 , 2012 , Pages 82-89 ; 09215093 (ISSN) Hosseini Monazzah, A ; Bagheri, R ; Seyed Reihani, S. M ; Sharif University of Technology
    2012
    Abstract
    Damage tolerance improvement has been reported by laminating aluminum alloys and composites by researchers. Three-layer laminates comprising Al6061 outer layers and Al1050 interlayer have been roll bonded in this research. While most of the works done have focused on fracture properties of roll bonded Al laminates in crack arrester geometry, this study explores their behavior in crack divider configuration. Rolling strain is varied to control the interfacial bonding in laminates. The fracture behavior of laminates and the constituent material was examined via three-point bending and impact tests. This study presents significant improvement in damage tolerance of laminates compared to their...