    Hydrometallurgical treatment of tailings with high zinc content

    , Article Hydrometallurgy ; Volume 82, Issue 1-2 , 2006 , Pages 54-62 ; 0304386X (ISSN) Espiari, S ; Rashchi, F ; Sadrnezhaad, S. K ; Sharif University of Technology
    2006
    Abstract
    Zinc exists as smithsonite and hemimorphite in the lead flotation tailings from the Dandi mineral processing plant in north western Iran. In this research, zinc-rich tailings produced in the Dandi plant were characterized mineralogically and a leaching study was carried out to assess the effect of several parameters on the kinetics of zinc dissolution. Parameters studied included: sulfuric acid concentration, reaction time, temperature and slurry density. It was found that leaching is controlled by a single rate-controlling step with an activation energy of 23.5 kJ/mol. To overcome some of the filtration problems associated with polymerization of silicic acid, lime was added as a coagulant.... 

    Gold extraction from an oxide ore in iodine-iodide solutions

    , Article Industrial Electrochemistry and Electrochemical Engineering General Session - 220th ECS Meeting, Boston, MA, 9 October 2011 through 14 October 2011 ; Volume 41, Issue 17 , 2012 , Pages 53-60 ; 19385862 (ISSN) ; 9781607683070 (ISBN) Baghalha, M ; Sharif University of Technology
    Abstract
    Two types of gold ores were subjected to iodide/iodine leaching at room temperature. The effects of three factors, including ore type (a carbonaceous and an oxide gold ores), iodide/iodine concentration, and the presence of oxygen in solution on gold leaching performance were investigated. The carbonaceous ore showed only 20% gold extraction into the solution; since gold-iodide complexes would readily adsorb on organic matter. In contrast, gold extraction from the oxide ore in a solution containing 20 g/L iodide and 4 g/L iodine reached 77% in 6 h and 89% in 24 h. With iodate as the oxidant, no gold could be leached in 48 hours. When the iodate was partially converted to iodine by adding HCl... 

    The leaching kinetics of an oxide gold ore with iodide/iodine solutions

    , Article Hydrometallurgy ; Volume 113-114 , 2012 , Pages 42-50 ; 0304386X (ISSN) Baghalha, M ; Sharif University of Technology
    2012
    Abstract
    Two types of gold ores were subjected to iodide/iodine leaching at room temperature. The effects of three factors, including ore type (a carbonaceous and an oxide gold ores), iodide/iodine concentration, and the presence of oxygen in solution on gold leaching performance were investigated. The carbonaceous ore showed only 20% gold extraction, since gold-iodide complexes readily adsorb on organic matter. In contrast, gold extraction from the oxide ore in a solution containing 20 g/L iodide and 4 g/L iodine reached 77% in 6 h and 89% in 24 h. With iodate as the oxidant, no gold could be leached in 48 h. When the iodate was partially converted to iodine by adding HCl to the solution, gold...