Optimization and Kinetics of the Leaching of Titanium from Ilmenite and its Slag, M.Sc. Thesis Sharif University of Technology ; Halali, Mohammad (Supervisor)
Abstract
To obtain solutions containing Titanium, leaching of Ilmenite Concentrate of Kahnooj and its Slag by Sulfuric Acid 98% in various Conditions are Studied. Screening tests by Fractional Factorial method were designed, at this step effects of Temperature, Acid Concentration, Particle Size, Solid to liquid Ratio, Time and Stirring Speed were investigated and It was Concluded that Temperature, Time, Acid Concentration and Particle Size were the effective Parameters in both leaching process of Ilmenite and Slag. The Temperature, Time and Acid concentration had positive effect, whereas the Particle Size had negative effect. After screening step, effective parameters were optimized by Rotatable...
Cataloging briefOptimization and Kinetics of the Leaching of Titanium from Ilmenite and its Slag, M.Sc. Thesis Sharif University of Technology ; Halali, Mohammad (Supervisor)
Abstract
To obtain solutions containing Titanium, leaching of Ilmenite Concentrate of Kahnooj and its Slag by Sulfuric Acid 98% in various Conditions are Studied. Screening tests by Fractional Factorial method were designed, at this step effects of Temperature, Acid Concentration, Particle Size, Solid to liquid Ratio, Time and Stirring Speed were investigated and It was Concluded that Temperature, Time, Acid Concentration and Particle Size were the effective Parameters in both leaching process of Ilmenite and Slag. The Temperature, Time and Acid concentration had positive effect, whereas the Particle Size had negative effect. After screening step, effective parameters were optimized by Rotatable...
Find in contentBookmark |
|