Quantum dot-polymer hybrid nanomaterials in nanomedicine
Adeli, M ; Sharif University of Technology | 2012
110
Viewed
- Type of Document: Article
- Publisher: Nova Science Publishers, Inc , 2012
- Abstract:
- Semiconductor quantum dots are a new class of nanomaterials which have unique optical and electronic properties. Their novel properties promise them as candidates to use in many area of science such as nanomedicine. In this chapter, properties of quantum dots, their synthetic procedures, modification of their surface especially by polymers will be reviewed briefly. Biomedical applications of polymer-quantum dots and their toxicity concerns in biology and also strategies to reduce their toxicity will be discussed
- Keywords:
- Source: Hybrid Nanostructures in Cancer Therapy ; 2012 , Pages 115-136 ; 9781621005179 (ISBN)
- URL: https://www.novapublishers.com/catalog/product_info.php?products_id=29121&osCsid