Loading...

Corrigendum to “Adsorptive desulfurization of wild naphtha using magnesium hydroxide-coated ceramic foam filters in pilot scale: Process optimization and sensitivity analysis” [Chem. Eng. Process.: Process Intensif. 152 (2020) 107937] (Chemical Engineering and Processing - Process Intensification (2020) 152, (S0255270120303949), (10.1016/j.cep.2020.107937))

Salehi, E ; Sharif University of Technology | 2020

68 Viewed
  1. Type of Document: Article
  2. DOI: 10.1016/j.cep.2020.107986
  3. Publisher: Elsevier B.V , 2020
  4. Abstract:
  5. The authors regret to inform that an error occurred in the arrangement and display of three figures (Figs. 3, 4 and 5) of the article with the aforementioned title [1]. These figures are related to the binary interaction curves of the operating variables and the results of the sensitivity analyses. The correct figures are now presented via this corrigendum. It is worth mentioning that none of these mistakes affect the originality of the article's text and the presented results. The authors would like to apologise for any inconvenience caused. [1] E. Salehi, M. Askari, S. Afshar, B. Eidi, M. H. Aliee, Adsorptive Desulfurization of Wild Naphtha Using Magnesium Hydroxide – Coated Ceramic Foams in Pilot Scale: Process Optimization and Sensitivity Analysis, Chemical Engineering and Processing: Process Intensification 152 (2020) 107937 Figure 3 3D plots for determination of interactive effects of operating parameters on sulfur removal. [Figure presented] Figure 4 Sensitivity of sulfur removal to the operating variables. [Figure presented] Figure 5 Scatter plots for determination of variations of sulfur removal with (a) temperature (b) pressure (c) adsorption bed length (d) initial sulfur concentration. [Figure presented] © 2020
  6. Keywords:
  7. Source: Chemical Engineering and Processing - Process Intensification ; Volume 153 , 2020
  8. URL: https://www.sciencedirect.com/science/article/pii/S0255270120304438