Tensile deformation mechanisms at different temperatures in the Ni-base superalloy GTD-111
Sajjadi, S. A
Cataloging brief
Tensile deformation mechanisms at different temperatures in the Ni-base superalloy GTD-111
Author :
Sajjadi, S. A
Publisher :
Pub. Year :
2004
Subjects :
γ precipitates GTD-111 superalloy TEM Tensile behavior